Author: Walter F. Czyrklis
Publisher:
ISBN:
Category :
Languages : en
Pages : 17
Book Description
The study was carried out to determine the critical threshold intensity for stress corrosion cracking of several uranium alloys which are candidates for ballistic penetrator and nuclear shell applications. The data reported here are for alloys in the as-extruded condition only and will serve as base-line data for future studies involving the solution-treated-and-aged alloys.
Stress Corrosion Cracking of Uranium Alloys
Stress Corrosion of Uranium Alloys
A Survey of Factors which Influence Stress Corrosion Crack Initiation in Several Uranium Base Alloys
Author: L. L. Stephenson
Publisher:
ISBN:
Category : Stress corrosion
Languages : en
Pages : 30
Book Description
Publisher:
ISBN:
Category : Stress corrosion
Languages : en
Pages : 30
Book Description
Stress Corrosion Cracking in Uranium Molybdenum Alloys
Author: John Warren Pridgeon
Publisher:
ISBN:
Category : Molybdenum alloys
Languages : en
Pages : 150
Book Description
Publisher:
ISBN:
Category : Molybdenum alloys
Languages : en
Pages : 150
Book Description
Electrochemical and Other Studies of a Uranium Alloy Exhibiting Stress-corrosion Cracking
Stress Corrosion Cracking of Uranium--niobium Alloys
Author:
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
The stress corrosion cracking behavior of U-21/4, 41/2, 6 and 8 wt % Nb alloys was evaluated in laboratory air and in aqueous Cl− solutions. Thresholds for crack propagation were obtained in these environments. The data showed that Cl− solutions are more deleterious than air environments. Tests were also conducted in pure gases to identify the species in the air responsible for cracking. These data showed the primary stress corrodent is water vapor for the most reactive alloy, U-21/4% Nb, while O2 is primarily responsible for cracking in the more corrosion resistant alloys, U-6 and 8% Nb. The 41/2% alloy was found to be susceptible in both H2O and O2 environments.
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
The stress corrosion cracking behavior of U-21/4, 41/2, 6 and 8 wt % Nb alloys was evaluated in laboratory air and in aqueous Cl− solutions. Thresholds for crack propagation were obtained in these environments. The data showed that Cl− solutions are more deleterious than air environments. Tests were also conducted in pure gases to identify the species in the air responsible for cracking. These data showed the primary stress corrodent is water vapor for the most reactive alloy, U-21/4% Nb, while O2 is primarily responsible for cracking in the more corrosion resistant alloys, U-6 and 8% Nb. The 41/2% alloy was found to be susceptible in both H2O and O2 environments.
A Comparison of the Corrosion and Stress Corrosion Resistance of Two Depleted Uranium Alloys; DU-0.75 Ti and DU-2 Mo
Author: Patricia P. Trzaskoma
Publisher:
ISBN:
Category :
Languages : en
Pages : 17
Book Description
Considerable experimental work concerning the corrosion rates, stress corrosion behavior, and effects of corrosion on the mechanical properties of depleted uranium alloys has been performed. In this study data for two alloys, DU-0.75 Ti and DU-2 Mo, in three environments have been collected and compared in order to determine whether there are significant differences in their corrosion characteristics and whether these differences warrant a choice of alloy for kinetic energy penetrator applications. In moist air the corrosion rates of the two alloys are low and appear to be of little consequence with respect to this application. In salt fog the corrosion rate of DU-3/4 Ti increases sharply. The weight loss in thirty days is about 7% of the total weight. No data was found for the molybdenum alloy in salt fog. Further experimental work is suggested.
Publisher:
ISBN:
Category :
Languages : en
Pages : 17
Book Description
Considerable experimental work concerning the corrosion rates, stress corrosion behavior, and effects of corrosion on the mechanical properties of depleted uranium alloys has been performed. In this study data for two alloys, DU-0.75 Ti and DU-2 Mo, in three environments have been collected and compared in order to determine whether there are significant differences in their corrosion characteristics and whether these differences warrant a choice of alloy for kinetic energy penetrator applications. In moist air the corrosion rates of the two alloys are low and appear to be of little consequence with respect to this application. In salt fog the corrosion rate of DU-3/4 Ti increases sharply. The weight loss in thirty days is about 7% of the total weight. No data was found for the molybdenum alloy in salt fog. Further experimental work is suggested.
STRESS CORROSION CRACKING IN URANIUM-MOLYBDENUM ALLOYS.
Author:
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
An investigation was conducted to determine the cause of cracking, during tension, on the surface of tensile specimens of U--Mo alloys. The cracking was observed in alloys that were water quenched from a temperature range in which the body-centered cubic gamma phase was stable and, subsequently, stressed in tension. The investigation was carried out on alloys of U--Mo containing 5 and 4 wt% Mo. It was discovered early in the study that the cracking could be eliminated by testing tensile specimens in a He atmosphere. Because of this result, tensile tests were performed in vacuum O22, impure N2, and purified N2. Additional experiments were done to establish the relation of stress state, temperature, strain rate, O2 pressure, stress magnitude, and grain size to the cracking phenomenon. U--4 wt% Mo and U--5 wt% Mo were compared with respect to microstructure and crystal structure, since both alloys cracked during the tensile test. The origin and propagation of cracks in the microstructure were studied, using motion pictures and metallography. The results of the various experiments showed that the cracking occurred only in tension and was caused by stress-corrosion cracking due to the presence of O/sub 2/ in the atmosphere. The rate of cracking increased as the temperature was increased above 25 deg C. Below 10 deg C cracking was not observed in the U-5 wt% Mo alloy. Cracking was not associated with just one metastable phase. since it was observed in both the U-5 wt% Mo and U-4 wt% Mo alloys, which have different crystal structures when rendered metastable by water quenching from the gamma phase field. The path of fracture was transgranular and was not associated with deformation markings in the grains. (auth).
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
An investigation was conducted to determine the cause of cracking, during tension, on the surface of tensile specimens of U--Mo alloys. The cracking was observed in alloys that were water quenched from a temperature range in which the body-centered cubic gamma phase was stable and, subsequently, stressed in tension. The investigation was carried out on alloys of U--Mo containing 5 and 4 wt% Mo. It was discovered early in the study that the cracking could be eliminated by testing tensile specimens in a He atmosphere. Because of this result, tensile tests were performed in vacuum O22, impure N2, and purified N2. Additional experiments were done to establish the relation of stress state, temperature, strain rate, O2 pressure, stress magnitude, and grain size to the cracking phenomenon. U--4 wt% Mo and U--5 wt% Mo were compared with respect to microstructure and crystal structure, since both alloys cracked during the tensile test. The origin and propagation of cracks in the microstructure were studied, using motion pictures and metallography. The results of the various experiments showed that the cracking occurred only in tension and was caused by stress-corrosion cracking due to the presence of O/sub 2/ in the atmosphere. The rate of cracking increased as the temperature was increased above 25 deg C. Below 10 deg C cracking was not observed in the U-5 wt% Mo alloy. Cracking was not associated with just one metastable phase. since it was observed in both the U-5 wt% Mo and U-4 wt% Mo alloys, which have different crystal structures when rendered metastable by water quenching from the gamma phase field. The path of fracture was transgranular and was not associated with deformation markings in the grains. (auth).
Stress-corrosion Cracking
Author: Russell H. Jones
Publisher: ASM International(OH)
ISBN:
Category : Science
Languages : en
Pages : 466
Book Description
Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen
Publisher: ASM International(OH)
ISBN:
Category : Science
Languages : en
Pages : 466
Book Description
Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen