Author:
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
The most recent corrosion problems experienced in nuclear steam generators tubed with Inconel alloy 600 is a phenomenon labeled ''denting''. Denting has been found in various degrees of severity in many operating pressurized water reactors. Laboratory investigations have shown that Inconel 600 exhibits intergranular SCC when subjected to high stresses and exposed to deoxygenated water at elevated temperatures. A research project was initiated at Brookhaven National Laboratory in an attempt to improve the qualitative and quantitative understanding of factors influencing SCC in high temperature service-related environments. An effort is also being made to develop an accelerated test method which could be used to predict the service life of tubes which have been deformed or are actively denting. Several heats of commercial Inconel 600 tubing were procured for testing in deaerated pure and primary water at temperatures from 290 to 365/sup 0/C. U-bend type specimens were used to determine crack initiation times which may be expected for tubes where denting has occurred but is arrested and provide baseline data for judging the accelerating effects of the slow strain rate method. Constant extension rate tests were employed to determine the crack velocities experienced in the crack propagation stage and predict failure times of tubes which are actively denting. 8 refs., 17 figs., 5 tabs.
Stress Corrosion Cracking of Alloy 600 Using the Constant Strain Rate Test
Stress Corrosion Cracking--the Slow Strain-rate Technique
Author: National Association of Corrosion Engineers. TPC Committee T-3E on Stress Corrosion Cracking of Metallic Materials
Publisher: Philadelphia : ASTM
ISBN:
Category : Technology & Engineering
Languages : en
Pages : 460
Book Description
Publisher: Philadelphia : ASTM
ISBN:
Category : Technology & Engineering
Languages : en
Pages : 460
Book Description
Stress Corrosion Cracking-the Slow Strain-rate Technique
Author: G. M. Ugiansky
Publisher: ASTM International
ISBN:
Category :
Languages : en
Pages : 446
Book Description
Publisher: ASTM International
ISBN:
Category :
Languages : en
Pages : 446
Book Description
Slow Strain-Rate Technique
Author: GJ. Theus
Publisher:
ISBN:
Category : Alloys
Languages : en
Pages : 16
Book Description
This paper describes slow strain-rate test equipment, operable at elevated temperatures and pressures, that includes electrochemical potential control capability. Applications in caustic stress corrosion cracking (SCC) studies of both nuclear steam generator and fossil boiler materials are presented. Electrochemical potential regions for stress corrosion cracking of Inconel alloy 600, Incoloy alloy 800, and Type 304 stainless steel are compared to results obtained using constant load specimens. Tests with titanium stabilized Alloy 800 (Sanicro 30) tubular specimens also demonstrate the effect of potential on cracking mode. A comparison of SCC test results, using both long term exposure tests and short term straining electrode tests, is made between a mild steel and its weld metal. In these examples, favorable comparisons are obtained with tests using conventional methods, proving the value and usefulness of the slow straining device in accelerating SCC studies and in defining more accurately conditions under which SCC can occur.
Publisher:
ISBN:
Category : Alloys
Languages : en
Pages : 16
Book Description
This paper describes slow strain-rate test equipment, operable at elevated temperatures and pressures, that includes electrochemical potential control capability. Applications in caustic stress corrosion cracking (SCC) studies of both nuclear steam generator and fossil boiler materials are presented. Electrochemical potential regions for stress corrosion cracking of Inconel alloy 600, Incoloy alloy 800, and Type 304 stainless steel are compared to results obtained using constant load specimens. Tests with titanium stabilized Alloy 800 (Sanicro 30) tubular specimens also demonstrate the effect of potential on cracking mode. A comparison of SCC test results, using both long term exposure tests and short term straining electrode tests, is made between a mild steel and its weld metal. In these examples, favorable comparisons are obtained with tests using conventional methods, proving the value and usefulness of the slow straining device in accelerating SCC studies and in defining more accurately conditions under which SCC can occur.
Slow Strain Rate Testing for the Evaluation of Environmentally Induced Cracking
Author: R. D. Kane
Publisher: ASTM International
ISBN: 0803118708
Category : Alloys
Languages : en
Pages : 298
Book Description
In order to predict when and how a material will crack under environmental conditions, engineers used to subject it to pressure for a long time, up to a year in cases; about 20 years ago, a testing method was developed that slowly but inexorably increases the pressure, which seems to cut down the ti
Publisher: ASTM International
ISBN: 0803118708
Category : Alloys
Languages : en
Pages : 298
Book Description
In order to predict when and how a material will crack under environmental conditions, engineers used to subject it to pressure for a long time, up to a year in cases; about 20 years ago, a testing method was developed that slowly but inexorably increases the pressure, which seems to cut down the ti
A Review of the Constant Strain-Rate Stress Corrosion Cracking Test
Author: CD. Kim
Publisher:
ISBN:
Category : Alloys
Languages : en
Pages : 16
Book Description
A review of six years operational experience in using the slow strain test procedure has indicated several unique advantages associated with dynamic strain techniques and also identified an area of limitation.
Publisher:
ISBN:
Category : Alloys
Languages : en
Pages : 16
Book Description
A review of six years operational experience in using the slow strain test procedure has indicated several unique advantages associated with dynamic strain techniques and also identified an area of limitation.
Energy Research Abstracts
A Stress Corrosion Cracking Test with Slow Strain Rate and Constant Current
Stress Corrosion Crack Nucleation in Alloy 600 and the Effect of Surface Modification
Stress Corrosion Cracking Test with Slow Strain Rate and Constant Current
Author: RS. Ondrejcin
Publisher:
ISBN:
Category : Alloys
Languages : en
Pages : 19
Book Description
A rapid electrochemical tension test was developed for evaluating stress corrosion crack initiation in carbon steel. Constant anodic current was imposed on smooth-bar tension specimens as the specimens were slowly strained to fracture at 1.3 x 10-6/s. Equivalent results were obtained for the following ductility properties measured: uniform elongation, total elongation, and reduction of area. Total elongation was chosen as the index for stress corrosion crack initiation. An equation was developed that allowed calculation of total elongation of specimens in electrolytes (test solutions) with composition ranges of 1.5 to 5.5 M nitrate, 0 to 3.5 M nitrite, and 0 to 5.0 M hydroxide, and a temperature range of 50 to 100°C. A minimum of 13 percent total elongation was selected to indicate the possible initiation of cracking in A 285-B steel alloy.
Publisher:
ISBN:
Category : Alloys
Languages : en
Pages : 19
Book Description
A rapid electrochemical tension test was developed for evaluating stress corrosion crack initiation in carbon steel. Constant anodic current was imposed on smooth-bar tension specimens as the specimens were slowly strained to fracture at 1.3 x 10-6/s. Equivalent results were obtained for the following ductility properties measured: uniform elongation, total elongation, and reduction of area. Total elongation was chosen as the index for stress corrosion crack initiation. An equation was developed that allowed calculation of total elongation of specimens in electrolytes (test solutions) with composition ranges of 1.5 to 5.5 M nitrate, 0 to 3.5 M nitrite, and 0 to 5.0 M hydroxide, and a temperature range of 50 to 100°C. A minimum of 13 percent total elongation was selected to indicate the possible initiation of cracking in A 285-B steel alloy.