Author: ANDREW LEE PURVIS
Publisher:
ISBN:
Category :
Languages : en
Pages : 219
Book Description
attributed to data scatter and the simultaneous generation of acoustic emission signals for a number of these sources.
THE ACOUSTIC EMISSION CHARACTERISTICS OF SOLIDIFICATION AND FORMATION OF CASTING DEFECTS IN ALUMINUM ALLOY 319
Author: ANDREW LEE PURVIS
Publisher:
ISBN:
Category :
Languages : en
Pages : 219
Book Description
attributed to data scatter and the simultaneous generation of acoustic emission signals for a number of these sources.
Publisher:
ISBN:
Category :
Languages : en
Pages : 219
Book Description
attributed to data scatter and the simultaneous generation of acoustic emission signals for a number of these sources.
Scientific and Technical Aerospace Reports
Transactions of the American Foundrymen's Society
Author: American Foundrymen's Society
Publisher:
ISBN:
Category : Founding
Languages : en
Pages : 992
Book Description
Publisher:
ISBN:
Category : Founding
Languages : en
Pages : 992
Book Description
Metals Abstracts
American Doctoral Dissertations
Author:
Publisher:
ISBN:
Category : Dissertation abstracts
Languages : en
Pages : 768
Book Description
Publisher:
ISBN:
Category : Dissertation abstracts
Languages : en
Pages : 768
Book Description
The Effect of Solidification Time on the Mechanical Properties of a Cast 319 Aluminum Alloy
Meeting of Board of Regents
Author: University of Michigan. Board of Regents
Publisher:
ISBN:
Category :
Languages : en
Pages : 448
Book Description
Publisher:
ISBN:
Category :
Languages : en
Pages : 448
Book Description
Vibrations in Physical Systems
Solidification Characteristics of Aluminum Alloys
Acoustic Emission from the Aluminium Alloy 7050
Author: S. McK. Cousland
Publisher:
ISBN: 9780642891020
Category : Acoustic emission
Languages : en
Pages : 26
Book Description
Studies of the acoustic emission detected during deformation of the commercial aluminum alloy 7050 are described. Tests have been performed on unflawed tensile specimens and notched specimens of the alloy in a variety of heat-treated conditions. Attempts are made to correlate the detected emission with various microstructural features affecting the deformation of the alloy. (Author).
Publisher:
ISBN: 9780642891020
Category : Acoustic emission
Languages : en
Pages : 26
Book Description
Studies of the acoustic emission detected during deformation of the commercial aluminum alloy 7050 are described. Tests have been performed on unflawed tensile specimens and notched specimens of the alloy in a variety of heat-treated conditions. Attempts are made to correlate the detected emission with various microstructural features affecting the deformation of the alloy. (Author).