Book Description
Fuel Performance Improvement Program
Research on Mechanisms of Stress Corrosion Cracking in Zircaloy
Author:
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
The results of internal gas pressurization tests, primarily at 320°C, on cladding tubes from two suppliers, Supplier A and Supplier B, are presented. The two lots show a substantial difference in iodine SCC susceptibility so a test matrix is used to resolve the relative contributions of surface condition, residual stress, and texture. Additional tests with constant deflection split-ring specimens and with unstressed cladding segments are used to understand crack initiation and the early crack growth stages of SCC. The difference in SCC susceptibility is due to crystallographic texture. Other variables such as surface finish, stress relief temperature, and residual stress have little or no effect. Mechanical properties, crack initiation, and crack propagation all depend on texture. Both initiation and propagation features are analyzed by scanning electron microscopy. A mechanism for crack initiation consistent with most observations in this study and with the work of other investigators is proposed. At 320°C, lifetime is crack initiation limited while several tests at 390°C indicate that lifetime is less initiation limited at higher temperature. 31 figures, 9 tables.
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
The results of internal gas pressurization tests, primarily at 320°C, on cladding tubes from two suppliers, Supplier A and Supplier B, are presented. The two lots show a substantial difference in iodine SCC susceptibility so a test matrix is used to resolve the relative contributions of surface condition, residual stress, and texture. Additional tests with constant deflection split-ring specimens and with unstressed cladding segments are used to understand crack initiation and the early crack growth stages of SCC. The difference in SCC susceptibility is due to crystallographic texture. Other variables such as surface finish, stress relief temperature, and residual stress have little or no effect. Mechanical properties, crack initiation, and crack propagation all depend on texture. Both initiation and propagation features are analyzed by scanning electron microscopy. A mechanism for crack initiation consistent with most observations in this study and with the work of other investigators is proposed. At 320°C, lifetime is crack initiation limited while several tests at 390°C indicate that lifetime is less initiation limited at higher temperature. 31 figures, 9 tables.
Grain-by-Grain Study of the Mechanisms of Crack Propagation During Iodine Stress Corrosion Cracking of Zircaloy-4
Author: AO. Dorado
Publisher:
ISBN:
Category : Applied stress
Languages : en
Pages : 17
Book Description
This paper describes the tests conducted to determine the conditions leading to cracking of a specified grain of metal, during the iodine stress corrosion cracking (SCC) of zirconium alloys, focusing on the crystallographic orientation of crack paths, the critical stress conditions, and the significance of the fractographic features encountered. In order to perform crystalline orientation of fracture surfaces, a specially heat-treated Zircaloy-4 having very large grains, grown up to the wall thickness, was used. Careful orientation work has proved that intracrystalline pseudo-cleavage occurs only along basal planes. The effects of anisotropy, plasticity, triaxiality, and residual stresses originated in thermal contraction have to be considered to account for the influence of the stress state. A grain-by-grain calculation led to the conclusion that transgranular cracking always takes place on those bearing the maximum resolved tensile stress perpendicular to basal planes. Propagation along twin boundaries has been identified among the different fracture modes encountered.
Publisher:
ISBN:
Category : Applied stress
Languages : en
Pages : 17
Book Description
This paper describes the tests conducted to determine the conditions leading to cracking of a specified grain of metal, during the iodine stress corrosion cracking (SCC) of zirconium alloys, focusing on the crystallographic orientation of crack paths, the critical stress conditions, and the significance of the fractographic features encountered. In order to perform crystalline orientation of fracture surfaces, a specially heat-treated Zircaloy-4 having very large grains, grown up to the wall thickness, was used. Careful orientation work has proved that intracrystalline pseudo-cleavage occurs only along basal planes. The effects of anisotropy, plasticity, triaxiality, and residual stresses originated in thermal contraction have to be considered to account for the influence of the stress state. A grain-by-grain calculation led to the conclusion that transgranular cracking always takes place on those bearing the maximum resolved tensile stress perpendicular to basal planes. Propagation along twin boundaries has been identified among the different fracture modes encountered.
Stress Corrosion Cracking
Author: V S Raja
Publisher: Elsevier
ISBN: 0857093762
Category : Technology & Engineering
Languages : en
Pages : 817
Book Description
The problem of stress corrosion cracking (SCC), which causes sudden failure of metals and other materials subjected to stress in corrosive environment(s), has a significant impact on a number of sectors including the oil and gas industries and nuclear power production. Stress corrosion cracking reviews the fundamentals of the phenomenon as well as examining stress corrosion behaviour in specific materials and particular industries.The book is divided into four parts. Part one covers the mechanisms of SCC and hydrogen embrittlement, while the focus of part two is on methods of testing for SCC in metals. Chapters in part three each review the phenomenon with reference to a specific material, with a variety of metals, alloys and composites discussed, including steels, titanium alloys and polymer composites. In part four, the effect of SCC in various industries is examined, with chapters covering subjects such as aerospace engineering, nuclear reactors, utilities and pipelines.With its distinguished editors and international team of contributors, Stress corrosion cracking is an essential reference for engineers and designers working with metals, alloys and polymers, and will be an invaluable tool for any industries in which metallic components are exposed to tension, corrosive environments at ambient and high temperatures. - Examines the mechanisms of stress corrosion cracking (SCC) presenting recognising testing methods and materials resistant to SCC - Assesses the effect of SCC on particular metals featuring steel, stainless steel, nickel-based alloys, magnesium alloys, copper-based alloys and welds in steels - Reviews the monitoring and management of SCC and the affect of SCC in different industries such as petrochemical and aerospace
Publisher: Elsevier
ISBN: 0857093762
Category : Technology & Engineering
Languages : en
Pages : 817
Book Description
The problem of stress corrosion cracking (SCC), which causes sudden failure of metals and other materials subjected to stress in corrosive environment(s), has a significant impact on a number of sectors including the oil and gas industries and nuclear power production. Stress corrosion cracking reviews the fundamentals of the phenomenon as well as examining stress corrosion behaviour in specific materials and particular industries.The book is divided into four parts. Part one covers the mechanisms of SCC and hydrogen embrittlement, while the focus of part two is on methods of testing for SCC in metals. Chapters in part three each review the phenomenon with reference to a specific material, with a variety of metals, alloys and composites discussed, including steels, titanium alloys and polymer composites. In part four, the effect of SCC in various industries is examined, with chapters covering subjects such as aerospace engineering, nuclear reactors, utilities and pipelines.With its distinguished editors and international team of contributors, Stress corrosion cracking is an essential reference for engineers and designers working with metals, alloys and polymers, and will be an invaluable tool for any industries in which metallic components are exposed to tension, corrosive environments at ambient and high temperatures. - Examines the mechanisms of stress corrosion cracking (SCC) presenting recognising testing methods and materials resistant to SCC - Assesses the effect of SCC on particular metals featuring steel, stainless steel, nickel-based alloys, magnesium alloys, copper-based alloys and welds in steels - Reviews the monitoring and management of SCC and the affect of SCC in different industries such as petrochemical and aerospace
Stress-corrosion Cracking
Author: Russell H. Jones
Publisher: ASM International(OH)
ISBN:
Category : Science
Languages : en
Pages : 466
Book Description
Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen
Publisher: ASM International(OH)
ISBN:
Category : Science
Languages : en
Pages : 466
Book Description
Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen
Stress-corrosion cracking of zircaloy in iodine; a probable failure mechanism in water reactor fuel pins
A Possible Mechanism of Crack Initiation in Zirconium that Leads to Observed Stress Corrosion Cracking in Nuclear Fuel Rods
Author: Rajan Deshmukh
Publisher:
ISBN:
Category : Nuclear fuel rods
Languages : en
Pages : 54
Book Description
Publisher:
ISBN:
Category : Nuclear fuel rods
Languages : en
Pages : 54
Book Description
Stress Corrosion Cracking of Zirconium in Nitric Acid
Author:
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
The susceptibility of zirconium and its common alloys to stress corrosion cracking (SCC) in nitric acid was investigated by slow strain-rate and constant deflection techniques. Cracking occurred at 25°C over a wide range of acid concentrations and electrochemical potentials. The crack velocity increased slightly with increasing temperature. The failure mode was transgranular and the morphology was similar to SCC failures of zirconium alloys in other environments. The fracture was very orientation-dependent suggesting that it occurs on a single crystallographic plane in the material. The results of the study are not consistent with a hydrogen mechanism for cracking.
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
The susceptibility of zirconium and its common alloys to stress corrosion cracking (SCC) in nitric acid was investigated by slow strain-rate and constant deflection techniques. Cracking occurred at 25°C over a wide range of acid concentrations and electrochemical potentials. The crack velocity increased slightly with increasing temperature. The failure mode was transgranular and the morphology was similar to SCC failures of zirconium alloys in other environments. The fracture was very orientation-dependent suggesting that it occurs on a single crystallographic plane in the material. The results of the study are not consistent with a hydrogen mechanism for cracking.
Failure Mechanisms of Irradiated Zr Alloys Related to PCI
Author: L. Rouillon
Publisher:
ISBN:
Category : Deformation
Languages : en
Pages : 22
Book Description
The impact of irradiation damage accumulated in fuel claddings on their mechanical behavior and their susceptibility to iodine-induced stress corrosion cracking (I-SCC) was studied in irradiated zirconium and standard Zircaloy-4 sheets subjected to interrupted tension tests in methanol/iodine solutions and in an inert environment. The study of the I-SCC cracks has been carried out by SEM, while the characterization of the irradiation defects and the activated slip systems used TEM.
Publisher:
ISBN:
Category : Deformation
Languages : en
Pages : 22
Book Description
The impact of irradiation damage accumulated in fuel claddings on their mechanical behavior and their susceptibility to iodine-induced stress corrosion cracking (I-SCC) was studied in irradiated zirconium and standard Zircaloy-4 sheets subjected to interrupted tension tests in methanol/iodine solutions and in an inert environment. The study of the I-SCC cracks has been carried out by SEM, while the characterization of the irradiation defects and the activated slip systems used TEM.
Potential Corrosion and Degradation Mechanisms of Zircaloy Cladding on Spent Nuclear Fuel in a Tuff Repository
Author:
Publisher:
ISBN:
Category :
Languages : en
Pages : 53
Book Description
A literature review and analysis were made of corrosion and degradation processes applicable to Zircaloy cladding on spent nuclear fuel in a tuff repository. In particular, lifetime sought for the Zircaloy is 10,000 years. Among the potential failure mechanisms examined were: oxidation by steam, air, and water, including the effects of ions whose presence is anticipated in the water; mechanical overload; stress (creep) rupture; stress-corrosion cracking (SCC); and delayed failure due to hydride cracking. The conclusion is that failure due to oxidation is not credible, although a few experiments are suggested to confirm the effect of aqueous fluoride on the Zircaloy cladding. Mechanical overload is not a problem, and failure from stress-rupture does not appear likely based on a modified Larson-Miller analysis. Analysis shows that delayed hydride cracking is not anticipated for the bulk of spent fuel pins. However, for a minority of pins under high stress, there is some uncertainty in the analysis as a result of: (1) uncertainty about crack depths in spent fuel claddings and (2) the effect of slow cooling on the formation of radially oriented hydride precipitates. Experimental resolution is called for. Finally, insufficient information is currently available on stress-corrosion cracking. While evidence is presented that SCC failure is not likely to occur, it is difficult to demonstrate this conclusively because the process is not clearly understood and data are limited. Further experimental work on SCC susceptibility is especially needed.
Publisher:
ISBN:
Category :
Languages : en
Pages : 53
Book Description
A literature review and analysis were made of corrosion and degradation processes applicable to Zircaloy cladding on spent nuclear fuel in a tuff repository. In particular, lifetime sought for the Zircaloy is 10,000 years. Among the potential failure mechanisms examined were: oxidation by steam, air, and water, including the effects of ions whose presence is anticipated in the water; mechanical overload; stress (creep) rupture; stress-corrosion cracking (SCC); and delayed failure due to hydride cracking. The conclusion is that failure due to oxidation is not credible, although a few experiments are suggested to confirm the effect of aqueous fluoride on the Zircaloy cladding. Mechanical overload is not a problem, and failure from stress-rupture does not appear likely based on a modified Larson-Miller analysis. Analysis shows that delayed hydride cracking is not anticipated for the bulk of spent fuel pins. However, for a minority of pins under high stress, there is some uncertainty in the analysis as a result of: (1) uncertainty about crack depths in spent fuel claddings and (2) the effect of slow cooling on the formation of radially oriented hydride precipitates. Experimental resolution is called for. Finally, insufficient information is currently available on stress-corrosion cracking. While evidence is presented that SCC failure is not likely to occur, it is difficult to demonstrate this conclusively because the process is not clearly understood and data are limited. Further experimental work on SCC susceptibility is especially needed.