Author:
Publisher:
ISBN:
Category :
Languages : en
Pages : 0
Book Description
Report of the U.S. Nuclear Regulatory Commission Piping Review Committee : investigation and evaluation of stress corrosion cracking in piping of boiling water reactor plants
Report of the US Nuclear Regulatory Commission Piping Review Committee. Volume 1. Investigation and Evaluation of Stress Corrosion Cracking in Piping of Boiling Water Reactor Plants
Author:
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
IGSCC in BWR piping is occurring owing to a combination of material, environment, and stress factors, each of which can affect both the initiation of a stress-corrosion crack and the rate of its subsequent propagation. In evaluating long-term solutions to the problem, one needs to consider the effects of each of the proposed remedial actions. Mitigating actions to control IGSCC in BWR piping must be designed to alleviate one or more of the three synergistic factors: sensitized material, the convention BWR environment, and high tensile stresses. Because mitigating actions addressing each of these factors may not be fully effective under all anticipated operating conditions, mitigating actions should address two and preferably all three of the causative factors; e.g., material plus some control of water chemistry, or stress reversal plus controlled water chemistry.
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
IGSCC in BWR piping is occurring owing to a combination of material, environment, and stress factors, each of which can affect both the initiation of a stress-corrosion crack and the rate of its subsequent propagation. In evaluating long-term solutions to the problem, one needs to consider the effects of each of the proposed remedial actions. Mitigating actions to control IGSCC in BWR piping must be designed to alleviate one or more of the three synergistic factors: sensitized material, the convention BWR environment, and high tensile stresses. Because mitigating actions addressing each of these factors may not be fully effective under all anticipated operating conditions, mitigating actions should address two and preferably all three of the causative factors; e.g., material plus some control of water chemistry, or stress reversal plus controlled water chemistry.
Report of the U.S. Nuclear Regulatory Commission Piping Review Committee
Author: U.S. Nuclear Regulatory Commission. Piping Review Committee. Pipe Crack Task Group
Publisher:
ISBN:
Category : Boiling water reactors
Languages : en
Pages : 418
Book Description
Publisher:
ISBN:
Category : Boiling water reactors
Languages : en
Pages : 418
Book Description
Report of the U.S. Nuclear Regulatory Commission Piping Review Committee: Evaluation of seismic designs: a review of seismic design requirements for nuclear power plant piping
Author: U.S. Nuclear Regulatory Commission. Piping Review Committee. Pipe Crack Task Group
Publisher:
ISBN:
Category : Boiling water reactors
Languages : en
Pages : 200
Book Description
Publisher:
ISBN:
Category : Boiling water reactors
Languages : en
Pages : 200
Book Description
Investigation and Evaluation of Stress-corrosion Cracking in Piping of Light Water Reactor Plants
Author: U.S. Nuclear Regulatory Commission
Publisher:
ISBN:
Category : Nuclear power plants
Languages : en
Pages : 116
Book Description
Publisher:
ISBN:
Category : Nuclear power plants
Languages : en
Pages : 116
Book Description
Report of the US Nuclear Regulatory Commission Piping Review Committee. Volume 5. Summary - Piping Review Committee Conclusions and Recommendations
Author:
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
This document summarizes a comprehensive review of NRC requirements for Nuclear Piping by the US NRC Piping Review Committee. Four topical areas, addressed in greater detail in Volumes 1 through 4 of this report, are included: (1) Stress Corrosion Cracking in Piping of Boiling Water Reactor Plants; (2) Evaluation of Seismic Design; (3) Evaluation of Potential for Pipe Breaks; and (4) Evaluation of Other Dynamic Loads and Load Combinations. This volume summarizes the major issues, reviews the interfaces, and presents the Committee's conclusions and recommendations for updating NRC requirements on these issues. This report also suggests research or other work that may be required to respond to issues not amenable to resolution at this time.
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
This document summarizes a comprehensive review of NRC requirements for Nuclear Piping by the US NRC Piping Review Committee. Four topical areas, addressed in greater detail in Volumes 1 through 4 of this report, are included: (1) Stress Corrosion Cracking in Piping of Boiling Water Reactor Plants; (2) Evaluation of Seismic Design; (3) Evaluation of Potential for Pipe Breaks; and (4) Evaluation of Other Dynamic Loads and Load Combinations. This volume summarizes the major issues, reviews the interfaces, and presents the Committee's conclusions and recommendations for updating NRC requirements on these issues. This report also suggests research or other work that may be required to respond to issues not amenable to resolution at this time.
Report of the U.S. Nuclear Regulatory Commission Piping Review Committee: Evaluation of seismic designs: a review of seismic design requirements for nuclear power plant piping
Author: U.S. Nuclear Regulatory Commission. Piping Review Committee. Pipe Crack Task Group
Publisher:
ISBN:
Category : Boiling water reactors
Languages : en
Pages : 222
Book Description
Publisher:
ISBN:
Category : Boiling water reactors
Languages : en
Pages : 222
Book Description
Investigation and Evaluation of Stress-corrosion Cracking in Piping of Boiling Water Reactor Plants
Author: U.S. Nuclear Regulatory Commission
Publisher:
ISBN:
Category : Boiling water reactors
Languages : en
Pages :
Book Description
Publisher:
ISBN:
Category : Boiling water reactors
Languages : en
Pages :
Book Description
Proceedings of the U.S. Nuclear Regulatory Commission Thirteenth Water Reactor Safety Research Information Meeting, Held at National Bureau of Standards, Gaithersburg, Maryland, October 22-25, 1985: Mechanical and structural research, Seismic research, Equipment qualification, Nuclear plan aging, Process control
Monthly Catalog of United States Government Publications
Author: United States. Superintendent of Documents
Publisher:
ISBN:
Category : Government publications
Languages : en
Pages :
Book Description
February issue includes Appendix entitled Directory of United States Government periodicals and subscription publications; September issue includes List of depository libraries; June and December issues include semiannual index
Publisher:
ISBN:
Category : Government publications
Languages : en
Pages :
Book Description
February issue includes Appendix entitled Directory of United States Government periodicals and subscription publications; September issue includes List of depository libraries; June and December issues include semiannual index