Author: M. Peehs
Publisher:
ISBN:
Category : Influence of stress
Languages : en
Pages : 17
Book Description
To investigate iodine stress corrosion cracking on the behavior of Zircaloy tubing, a standard test procedure with internally pressurized creep specimens (I-SCC standard test) and a split-ring test (I-SCC laboratory test) were developed. The threshold value for brittle cracking in iodine is 10-6 g iodine per square centimetre. The uniform elongation shows a clear minimum in its dependence on strain rate. Basal pole orientations in the range of ±50 to ±70 deg relative to the radial direction are the most I-SCC sensitive textures. The I-SCC process occurs in several stages; incubation, crack nucleation, and propagation. A thermodynamic evaluation indicates that I-SCC only occurs when zirconium iodides condense on the Zircaloy surface. Results show that comparisons of the I-SCC susceptibility of tubing manufactured in different manners should be made at the same point on the strain rate versus uniform elongation curves; for example, at the strain rate with the minimum of uniform elongation.
Out-of-Pile Testing of Iodine Stress Corrosion Cracking in Zircaloy Tubing in Relation to the Pellet-Cladding Interaction Phenomenon
Author: M. Peehs
Publisher:
ISBN:
Category : Influence of stress
Languages : en
Pages : 17
Book Description
To investigate iodine stress corrosion cracking on the behavior of Zircaloy tubing, a standard test procedure with internally pressurized creep specimens (I-SCC standard test) and a split-ring test (I-SCC laboratory test) were developed. The threshold value for brittle cracking in iodine is 10-6 g iodine per square centimetre. The uniform elongation shows a clear minimum in its dependence on strain rate. Basal pole orientations in the range of ±50 to ±70 deg relative to the radial direction are the most I-SCC sensitive textures. The I-SCC process occurs in several stages; incubation, crack nucleation, and propagation. A thermodynamic evaluation indicates that I-SCC only occurs when zirconium iodides condense on the Zircaloy surface. Results show that comparisons of the I-SCC susceptibility of tubing manufactured in different manners should be made at the same point on the strain rate versus uniform elongation curves; for example, at the strain rate with the minimum of uniform elongation.
Publisher:
ISBN:
Category : Influence of stress
Languages : en
Pages : 17
Book Description
To investigate iodine stress corrosion cracking on the behavior of Zircaloy tubing, a standard test procedure with internally pressurized creep specimens (I-SCC standard test) and a split-ring test (I-SCC laboratory test) were developed. The threshold value for brittle cracking in iodine is 10-6 g iodine per square centimetre. The uniform elongation shows a clear minimum in its dependence on strain rate. Basal pole orientations in the range of ±50 to ±70 deg relative to the radial direction are the most I-SCC sensitive textures. The I-SCC process occurs in several stages; incubation, crack nucleation, and propagation. A thermodynamic evaluation indicates that I-SCC only occurs when zirconium iodides condense on the Zircaloy surface. Results show that comparisons of the I-SCC susceptibility of tubing manufactured in different manners should be made at the same point on the strain rate versus uniform elongation curves; for example, at the strain rate with the minimum of uniform elongation.
Zirconium in the Nuclear Industry
Zirconium in the Nuclear Industry
Author: J. H. Schemel
Publisher: ASTM International
ISBN: 9780803106017
Category : Business & Economics
Languages : en
Pages : 656
Book Description
Publisher: ASTM International
ISBN: 9780803106017
Category : Business & Economics
Languages : en
Pages : 656
Book Description
Electrically Heated Ex-reactor Pellet-cladding Interaction (PCI) Simulations Utilizing Irradiated Zircaloy Cladding
Author: J. O. Barner
Publisher:
ISBN:
Category : Nuclear fuel claddings
Languages : en
Pages : 124
Book Description
Publisher:
ISBN:
Category : Nuclear fuel claddings
Languages : en
Pages : 124
Book Description
Pellet-cladding Interaction Failures in Water Reactor Fuel Rods
Author: Bernardo N. Nobrega
Publisher:
ISBN:
Category : Nuclear fuel claddings
Languages : en
Pages : 270
Book Description
Publisher:
ISBN:
Category : Nuclear fuel claddings
Languages : en
Pages : 270
Book Description
Energy Research Abstracts
Zirconium in the Nuclear Industry: Tenth International Symposium
Author: A. M. Garde
Publisher: ASTM International
ISBN: 0803120117
Category : Nuclear fuel claddings
Languages : en
Pages : 805
Book Description
Publisher: ASTM International
ISBN: 0803120117
Category : Nuclear fuel claddings
Languages : en
Pages : 805
Book Description
Pellet-clad Interaction in Water Reactor Fuels
Author:
Publisher: OECD Publishing
ISBN:
Category : Business & Economics
Languages : en
Pages : 562
Book Description
This publication sets out the findings of an international seminar, held in Aix-en-Provence, France in March 2004, which considered recent progress in the field of pellet-clad interaction in light water reactor fuels. It also reviews current understanding of relevant phenomena and their impact on the nuclear fuel rod under the widest possible conditions, and about both uranium-oxide and mixed-oxide fuels.
Publisher: OECD Publishing
ISBN:
Category : Business & Economics
Languages : en
Pages : 562
Book Description
This publication sets out the findings of an international seminar, held in Aix-en-Provence, France in March 2004, which considered recent progress in the field of pellet-clad interaction in light water reactor fuels. It also reviews current understanding of relevant phenomena and their impact on the nuclear fuel rod under the widest possible conditions, and about both uranium-oxide and mixed-oxide fuels.
Transactions of the 6th International Conference on Structural Mechanics in Reactor Technology, Palais Des Congres, Paris, France, 17-21 August 1981
Journal of Nuclear Science and Technology
Author:
Publisher:
ISBN:
Category : Nuclear energy
Languages : en
Pages : 1118
Book Description
Includes English language abstracts from Japanese articles in Nihon Genshiryoku Gakkai Shi (Journal of the Atomic Energy Society of Japan).
Publisher:
ISBN:
Category : Nuclear energy
Languages : en
Pages : 1118
Book Description
Includes English language abstracts from Japanese articles in Nihon Genshiryoku Gakkai Shi (Journal of the Atomic Energy Society of Japan).