Book Description
The gamma-gamma prime region of the nickel-aluminum-chromium-titanium system at 750' C has been analyzed through the use of phase rule principles and analytic geometry to allow estimation of gamma phase composition when the composition of a two-phase quaternary alloy is known. By application of currently used phase computation methods with the above calculation, the gamma phase composition of several nickel-base super-alloys was estimated and found (except for tungsten) to be in good agreement with compositions for these alloys as reported in the literature.
Estimation of Gamma Phase Composition in Nickel-base Superalloys (based on Geometric Analysis of a Four-component Phase Diagram)
Author: Robert L. Dreshfield
Publisher:
ISBN:
Category : Alloys
Languages : en
Pages : 28
Book Description
The gamma-gamma prime region of the nickel-aluminum-chromium-titanium system at 750' C has been analyzed through the use of phase rule principles and analytic geometry to allow estimation of gamma phase composition when the composition of a two-phase quaternary alloy is known. By application of currently used phase computation methods with the above calculation, the gamma phase composition of several nickel-base super-alloys was estimated and found (except for tungsten) to be in good agreement with compositions for these alloys as reported in the literature.
Publisher:
ISBN:
Category : Alloys
Languages : en
Pages : 28
Book Description
The gamma-gamma prime region of the nickel-aluminum-chromium-titanium system at 750' C has been analyzed through the use of phase rule principles and analytic geometry to allow estimation of gamma phase composition when the composition of a two-phase quaternary alloy is known. By application of currently used phase computation methods with the above calculation, the gamma phase composition of several nickel-base super-alloys was estimated and found (except for tungsten) to be in good agreement with compositions for these alloys as reported in the literature.
NASA Technical Note
Scientific and Technical Aerospace Reports
Monthly Catalogue, United States Public Documents
Author:
Publisher:
ISBN:
Category : Government publications
Languages : en
Pages : 1730
Book Description
Publisher:
ISBN:
Category : Government publications
Languages : en
Pages : 1730
Book Description
NASA Technical Memorandum
Bibliography of Lewis Research Center Technical Publications Announced in 1977
Author: Lewis Research Center
Publisher:
ISBN:
Category : Technology
Languages : en
Pages : 356
Book Description
This compilation of abstracts describes and indexes over 780 technical reports resulting from the scientific and engineering work performed and managed by the Lewis Research Center in 1977. All the publications were announced in the 1977 issues of STAR (Scientific and Technical Aerospace Reports) and/or IAA (International Aerospace Abstracts). Documents cited include research reports, journal articles, conference presentations, patents and patent applications, and theses.
Publisher:
ISBN:
Category : Technology
Languages : en
Pages : 356
Book Description
This compilation of abstracts describes and indexes over 780 technical reports resulting from the scientific and engineering work performed and managed by the Lewis Research Center in 1977. All the publications were announced in the 1977 issues of STAR (Scientific and Technical Aerospace Reports) and/or IAA (International Aerospace Abstracts). Documents cited include research reports, journal articles, conference presentations, patents and patent applications, and theses.
Monthly Catalog of United States Government Publications
Author: United States. Superintendent of Documents
Publisher:
ISBN:
Category : Government publications
Languages : en
Pages : 1464
Book Description
Publisher:
ISBN:
Category : Government publications
Languages : en
Pages : 1464
Book Description
The Aeronautical Journal
Monthly Catalog of United States Government Publications, Cumulative Index
Author: United States. Superintendent of Documents
Publisher:
ISBN:
Category : United States
Languages : en
Pages : 1504
Book Description
Publisher:
ISBN:
Category : United States
Languages : en
Pages : 1504
Book Description
The Effect of Alloying on Gamma and Gamma Prime in Nickel-base Superalloys
Author: Robert Lewis Dreshfield
Publisher:
ISBN:
Category :
Languages : en
Pages : 150
Book Description
Publisher:
ISBN:
Category :
Languages : en
Pages : 150
Book Description