Author: V S Raja
Publisher: Elsevier
ISBN: 0857093762
Category : Technology & Engineering
Languages : en
Pages : 817
Book Description
The problem of stress corrosion cracking (SCC), which causes sudden failure of metals and other materials subjected to stress in corrosive environment(s), has a significant impact on a number of sectors including the oil and gas industries and nuclear power production. Stress corrosion cracking reviews the fundamentals of the phenomenon as well as examining stress corrosion behaviour in specific materials and particular industries.The book is divided into four parts. Part one covers the mechanisms of SCC and hydrogen embrittlement, while the focus of part two is on methods of testing for SCC in metals. Chapters in part three each review the phenomenon with reference to a specific material, with a variety of metals, alloys and composites discussed, including steels, titanium alloys and polymer composites. In part four, the effect of SCC in various industries is examined, with chapters covering subjects such as aerospace engineering, nuclear reactors, utilities and pipelines.With its distinguished editors and international team of contributors, Stress corrosion cracking is an essential reference for engineers and designers working with metals, alloys and polymers, and will be an invaluable tool for any industries in which metallic components are exposed to tension, corrosive environments at ambient and high temperatures. - Examines the mechanisms of stress corrosion cracking (SCC) presenting recognising testing methods and materials resistant to SCC - Assesses the effect of SCC on particular metals featuring steel, stainless steel, nickel-based alloys, magnesium alloys, copper-based alloys and welds in steels - Reviews the monitoring and management of SCC and the affect of SCC in different industries such as petrochemical and aerospace
Stress Corrosion Cracking
Author: V S Raja
Publisher: Elsevier
ISBN: 0857093762
Category : Technology & Engineering
Languages : en
Pages : 817
Book Description
The problem of stress corrosion cracking (SCC), which causes sudden failure of metals and other materials subjected to stress in corrosive environment(s), has a significant impact on a number of sectors including the oil and gas industries and nuclear power production. Stress corrosion cracking reviews the fundamentals of the phenomenon as well as examining stress corrosion behaviour in specific materials and particular industries.The book is divided into four parts. Part one covers the mechanisms of SCC and hydrogen embrittlement, while the focus of part two is on methods of testing for SCC in metals. Chapters in part three each review the phenomenon with reference to a specific material, with a variety of metals, alloys and composites discussed, including steels, titanium alloys and polymer composites. In part four, the effect of SCC in various industries is examined, with chapters covering subjects such as aerospace engineering, nuclear reactors, utilities and pipelines.With its distinguished editors and international team of contributors, Stress corrosion cracking is an essential reference for engineers and designers working with metals, alloys and polymers, and will be an invaluable tool for any industries in which metallic components are exposed to tension, corrosive environments at ambient and high temperatures. - Examines the mechanisms of stress corrosion cracking (SCC) presenting recognising testing methods and materials resistant to SCC - Assesses the effect of SCC on particular metals featuring steel, stainless steel, nickel-based alloys, magnesium alloys, copper-based alloys and welds in steels - Reviews the monitoring and management of SCC and the affect of SCC in different industries such as petrochemical and aerospace
Publisher: Elsevier
ISBN: 0857093762
Category : Technology & Engineering
Languages : en
Pages : 817
Book Description
The problem of stress corrosion cracking (SCC), which causes sudden failure of metals and other materials subjected to stress in corrosive environment(s), has a significant impact on a number of sectors including the oil and gas industries and nuclear power production. Stress corrosion cracking reviews the fundamentals of the phenomenon as well as examining stress corrosion behaviour in specific materials and particular industries.The book is divided into four parts. Part one covers the mechanisms of SCC and hydrogen embrittlement, while the focus of part two is on methods of testing for SCC in metals. Chapters in part three each review the phenomenon with reference to a specific material, with a variety of metals, alloys and composites discussed, including steels, titanium alloys and polymer composites. In part four, the effect of SCC in various industries is examined, with chapters covering subjects such as aerospace engineering, nuclear reactors, utilities and pipelines.With its distinguished editors and international team of contributors, Stress corrosion cracking is an essential reference for engineers and designers working with metals, alloys and polymers, and will be an invaluable tool for any industries in which metallic components are exposed to tension, corrosive environments at ambient and high temperatures. - Examines the mechanisms of stress corrosion cracking (SCC) presenting recognising testing methods and materials resistant to SCC - Assesses the effect of SCC on particular metals featuring steel, stainless steel, nickel-based alloys, magnesium alloys, copper-based alloys and welds in steels - Reviews the monitoring and management of SCC and the affect of SCC in different industries such as petrochemical and aerospace
Stress Corrosion Cracking of Pipelines
Author: Y. Frank Cheng
Publisher: John Wiley & Sons
ISBN: 1118537084
Category : Science
Languages : en
Pages : 292
Book Description
Explains why pipeline stress corrosion cracking happens and how it can be prevented Pipelines sit at the heart of the global economy. When they are in good working order, they deliver fuel to meet the ever-growing demand for energy around the world. When they fail due to stress corrosion cracking, they can wreak environmental havoc. This book skillfully explains the fundamental science and engineering of pipeline stress corrosion cracking based on the latest research findings and actual case histories. The author explains how and why pipelines fall prey to stress corrosion cracking and then offers tested and proven strategies for preventing, detecting, and monitoring it in order to prevent pipeline failure. Stress Corrosion Cracking of Pipelines begins with a brief introduction and then explores general principals of stress corrosion cracking, including two detailed case studies of pipeline failure. Next, the author covers: Near-neutral pH stress corrosion cracking of pipelines High pH stress corrosion cracking of pipelines Stress corrosion cracking of pipelines in acidic soil environments Stress corrosion cracking at pipeline welds Stress corrosion cracking of high-strength pipeline steels The final chapter is dedicated to effective management and mitigation of pipeline stress corrosion cracking. Throughout the book, the author develops a number of theoretical models and concepts based on advanced microscopic electrochemical measurements to help readers better understand the occurrence of stress corrosion cracking. By examining all aspects of pipeline stress corrosion cracking—the causes, mechanisms, and management strategies—this book enables engineers to construct better pipelines and then maintain and monitor them to ensure safe, reliable energy supplies for the world.
Publisher: John Wiley & Sons
ISBN: 1118537084
Category : Science
Languages : en
Pages : 292
Book Description
Explains why pipeline stress corrosion cracking happens and how it can be prevented Pipelines sit at the heart of the global economy. When they are in good working order, they deliver fuel to meet the ever-growing demand for energy around the world. When they fail due to stress corrosion cracking, they can wreak environmental havoc. This book skillfully explains the fundamental science and engineering of pipeline stress corrosion cracking based on the latest research findings and actual case histories. The author explains how and why pipelines fall prey to stress corrosion cracking and then offers tested and proven strategies for preventing, detecting, and monitoring it in order to prevent pipeline failure. Stress Corrosion Cracking of Pipelines begins with a brief introduction and then explores general principals of stress corrosion cracking, including two detailed case studies of pipeline failure. Next, the author covers: Near-neutral pH stress corrosion cracking of pipelines High pH stress corrosion cracking of pipelines Stress corrosion cracking of pipelines in acidic soil environments Stress corrosion cracking at pipeline welds Stress corrosion cracking of high-strength pipeline steels The final chapter is dedicated to effective management and mitigation of pipeline stress corrosion cracking. Throughout the book, the author develops a number of theoretical models and concepts based on advanced microscopic electrochemical measurements to help readers better understand the occurrence of stress corrosion cracking. By examining all aspects of pipeline stress corrosion cracking—the causes, mechanisms, and management strategies—this book enables engineers to construct better pipelines and then maintain and monitor them to ensure safe, reliable energy supplies for the world.
Trends in Oil and Gas Corrosion Research and Technologies
Author: A. M. El-Sherik
Publisher: Woodhead Publishing
ISBN: 0081012195
Category : Science
Languages : en
Pages : 928
Book Description
Trends in Oil and Gas Corrosion Research and Technologies: Production and Transmission delivers the most up-to-date and highly multidisciplinary reference available to identify emerging developments, fundamental mechanisms and the technologies necessary in one unified source. Starting with a brief explanation on corrosion management that also addresses today's most challenging issues for oil and gas production and transmission operations, the book dives into the latest advances in microbiology-influenced corrosion and other corrosion threats, such as stress corrosion cracking and hydrogen damage just to name a few. In addition, it covers testing and monitoring techniques, such as molecular microbiology and online monitoring for surface and subsurface facilities, mitigation tools, including coatings, nano-packaged biocides, modeling and prediction, cathodic protection and new steels and non-metallics. Rounding out with an extensive glossary and list of abbreviations, the book equips upstream and midstream corrosion professionals in the oil and gas industry with the most advanced collection of topics and solutions to responsibly help solve today's oil and gas corrosion challenges. - Covers the latest in corrosion mitigation techniques, such as corrosion inhibitors, biocides, non-metallics, coatings, and modeling and prediction - Solves knowledge gaps with the most current technology and discoveries on specific corrosion mechanisms, highlighting where future research and industry efforts should be concentrated - Achieves practical and balanced understanding with a full spectrum of subjects presented from multiple academic and world-renowned contributors in the industry
Publisher: Woodhead Publishing
ISBN: 0081012195
Category : Science
Languages : en
Pages : 928
Book Description
Trends in Oil and Gas Corrosion Research and Technologies: Production and Transmission delivers the most up-to-date and highly multidisciplinary reference available to identify emerging developments, fundamental mechanisms and the technologies necessary in one unified source. Starting with a brief explanation on corrosion management that also addresses today's most challenging issues for oil and gas production and transmission operations, the book dives into the latest advances in microbiology-influenced corrosion and other corrosion threats, such as stress corrosion cracking and hydrogen damage just to name a few. In addition, it covers testing and monitoring techniques, such as molecular microbiology and online monitoring for surface and subsurface facilities, mitigation tools, including coatings, nano-packaged biocides, modeling and prediction, cathodic protection and new steels and non-metallics. Rounding out with an extensive glossary and list of abbreviations, the book equips upstream and midstream corrosion professionals in the oil and gas industry with the most advanced collection of topics and solutions to responsibly help solve today's oil and gas corrosion challenges. - Covers the latest in corrosion mitigation techniques, such as corrosion inhibitors, biocides, non-metallics, coatings, and modeling and prediction - Solves knowledge gaps with the most current technology and discoveries on specific corrosion mechanisms, highlighting where future research and industry efforts should be concentrated - Achieves practical and balanced understanding with a full spectrum of subjects presented from multiple academic and world-renowned contributors in the industry
Stress-corrosion Cracking
Author: Russell H. Jones
Publisher: ASM International(OH)
ISBN:
Category : Science
Languages : en
Pages : 466
Book Description
Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen
Publisher: ASM International(OH)
ISBN:
Category : Science
Languages : en
Pages : 466
Book Description
Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and testing for SCC, plus information on mechanisms of SCC with experimental data on a variety of materials. Contains information about environmen
Hydrogen Embrittlement and Stress Corrosion Cracking
Author: Alexander Robert Troiano
Publisher: ASM International
ISBN: 9781615031788
Category : Technology & Engineering
Languages : en
Pages : 356
Book Description
Publisher: ASM International
ISBN: 9781615031788
Category : Technology & Engineering
Languages : en
Pages : 356
Book Description
Atomistics of Fracture
Author: R.M. Latanison
Publisher: Springer Science & Business Media
ISBN: 1461335000
Category : Science
Languages : en
Pages : 1043
Book Description
It is now more than 100 years since certain detrimental effects on the ductility of iron were first associated with the presence of hydrogen. Not only is hydrogen embrittlement still a major industri al problem, but it is safe to say that in a mechanistic sense we still do not know what hydrogen (but not nitrogen or oxygen, for example) does on an atomic scale to induce this degradation. The same applies to other examples of environmentally-induced fracture: what is it about the ubiquitous chloride ion that induces premature catastrophic fracture (stress corrosion cracking) of ordinarily ductile austenitic stainless steels? Why, moreover, are halide ions troublesome but the nitrate or sulfate anions not deleterious to such stainless steels? Likewise, why are some solid metals embrit tled catastrophically by same liquid metals (liquid metal embrit tlement) - copper and aluminum, for example, are embrittled by liquid mercury. In short, despite all that we may know about the materials science and mechanics of fracture on a macroscopic scale, we know little about the atomistics of fracture in the absence of environmental interactions and even less when embrittlement phe nomena such as those described above are involved. On the other hand, it is interesting to note that physical chemists and surface chemists also have interests in the same kinds of interactions that occur on an atomic scale when metals such as nickel or platinum are used, for example, as catalysts for chemical reactions.
Publisher: Springer Science & Business Media
ISBN: 1461335000
Category : Science
Languages : en
Pages : 1043
Book Description
It is now more than 100 years since certain detrimental effects on the ductility of iron were first associated with the presence of hydrogen. Not only is hydrogen embrittlement still a major industri al problem, but it is safe to say that in a mechanistic sense we still do not know what hydrogen (but not nitrogen or oxygen, for example) does on an atomic scale to induce this degradation. The same applies to other examples of environmentally-induced fracture: what is it about the ubiquitous chloride ion that induces premature catastrophic fracture (stress corrosion cracking) of ordinarily ductile austenitic stainless steels? Why, moreover, are halide ions troublesome but the nitrate or sulfate anions not deleterious to such stainless steels? Likewise, why are some solid metals embrit tled catastrophically by same liquid metals (liquid metal embrit tlement) - copper and aluminum, for example, are embrittled by liquid mercury. In short, despite all that we may know about the materials science and mechanics of fracture on a macroscopic scale, we know little about the atomistics of fracture in the absence of environmental interactions and even less when embrittlement phe nomena such as those described above are involved. On the other hand, it is interesting to note that physical chemists and surface chemists also have interests in the same kinds of interactions that occur on an atomic scale when metals such as nickel or platinum are used, for example, as catalysts for chemical reactions.
Approximation of Free-Discontinuity Problems
Author: Andrea Braides
Publisher: Springer Science & Business Media
ISBN: 9783540647713
Category : Mathematics
Languages : en
Pages : 176
Book Description
Functionals involving both volume and surface energies have a number of applications ranging from Computer Vision to Fracture Mechanics. In order to tackle numerical and dynamical problems linked to such functionals many approximations by functionals defined on smooth functions have been proposed (using high-order singular perturbations, finite-difference or non-local energies, etc.) The purpose of this book is to present a global approach to these approximations using the theory of gamma-convergence and of special functions of bounded variation. The book is directed to PhD students and researchers in calculus of variations, interested in approximation problems with possible applications.
Publisher: Springer Science & Business Media
ISBN: 9783540647713
Category : Mathematics
Languages : en
Pages : 176
Book Description
Functionals involving both volume and surface energies have a number of applications ranging from Computer Vision to Fracture Mechanics. In order to tackle numerical and dynamical problems linked to such functionals many approximations by functionals defined on smooth functions have been proposed (using high-order singular perturbations, finite-difference or non-local energies, etc.) The purpose of this book is to present a global approach to these approximations using the theory of gamma-convergence and of special functions of bounded variation. The book is directed to PhD students and researchers in calculus of variations, interested in approximation problems with possible applications.
Stress-corrosion Cracking in High Strength Steels and in Titanium and Aluminum Alloys
Author: Benjamin Floyd Brown
Publisher:
ISBN:
Category : Aluminum alloys
Languages : en
Pages : 390
Book Description
Publisher:
ISBN:
Category : Aluminum alloys
Languages : en
Pages : 390
Book Description
Stress Corrosion Cracking of Metals-A State of the Art
Author: H. Lee Craig
Publisher: ASTM International
ISBN:
Category : Technology & Engineering
Languages : en
Pages : 184
Book Description
Publisher: ASTM International
ISBN:
Category : Technology & Engineering
Languages : en
Pages : 184
Book Description
Stress Corrosion Cracking Model for High Level Radioactive-Waste Packages
Author:
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
A stress corrosion cracking (SCC) model has been adapted for performance prediction of high level radioactive-waste packages to be emplaced in the proposed Yucca Mountain repository. For waste packages of the proposed Yucca Mountain repository, the outer barrier material is the highly corrosion-resistant Alloy UNS-N06022 (Alloy 22), the environment is represented by aqueous brine films present on the surface of the waste package from dripping or deliquescence of soluble salts present in any surface deposits, and the tensile stress is principally from weld induced residual stress. SCC has historically been separated into ''initiation'' and ''propagation'' phases. Initiation of SCC will not occur on a smooth surface if the surface stress is below a threshold value defined as the threshold stress. Cracks can also initiate at and propagate from flaws (or defects) resulting from manufacturing processes (such as welding); or that develop from corrosion processes such as pitting or dissolution of inclusions. To account for crack propagation, the slip dissolution/film rupture (SDFR) model is adopted to provide mathematical formulae for prediction of the crack growth rate. Once the crack growth rate at an initiated SCC is determined, it can be used by the performance assessment to determine the time to through-wall penetration for the waste package. This paper presents the development of the SDFR crack growth rate model based on technical information in the literature as well as experimentally determined crack growth rates developed specifically for Alloy UNS-N06022 in environments relevant to high level radioactive-waste packages of the proposed Yucca Mountain radioactive-waste repository. In addition, a seismic damage related SCC crack opening area density model is briefly described.
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
A stress corrosion cracking (SCC) model has been adapted for performance prediction of high level radioactive-waste packages to be emplaced in the proposed Yucca Mountain repository. For waste packages of the proposed Yucca Mountain repository, the outer barrier material is the highly corrosion-resistant Alloy UNS-N06022 (Alloy 22), the environment is represented by aqueous brine films present on the surface of the waste package from dripping or deliquescence of soluble salts present in any surface deposits, and the tensile stress is principally from weld induced residual stress. SCC has historically been separated into ''initiation'' and ''propagation'' phases. Initiation of SCC will not occur on a smooth surface if the surface stress is below a threshold value defined as the threshold stress. Cracks can also initiate at and propagate from flaws (or defects) resulting from manufacturing processes (such as welding); or that develop from corrosion processes such as pitting or dissolution of inclusions. To account for crack propagation, the slip dissolution/film rupture (SDFR) model is adopted to provide mathematical formulae for prediction of the crack growth rate. Once the crack growth rate at an initiated SCC is determined, it can be used by the performance assessment to determine the time to through-wall penetration for the waste package. This paper presents the development of the SDFR crack growth rate model based on technical information in the literature as well as experimentally determined crack growth rates developed specifically for Alloy UNS-N06022 in environments relevant to high level radioactive-waste packages of the proposed Yucca Mountain radioactive-waste repository. In addition, a seismic damage related SCC crack opening area density model is briefly described.